Repair of intense multiple cracks on plaster
Suggestions and solutions from ISOMAT!

Suggestions and solutions from ISOMAT!

1. Intense hair cracks on plaster may occur due to its wrong application (deficient dampening during summer months, lack of plaster reinforcement when applied on thermal-insulating boards etc.), as well as due to its bad quality.

2. Firstly, the surface needs to be cleaned of dust, etc.

3. Then, it is primed with FLEX-PRIMER follows. Especially when plasters are relatively unstable, FLEX-PRIMER is needed to stabilize their surfaces

4. FLEX-COVER is prepared by adding A-component into B-component under continuous stirring.

5. After the primer has dried, FLEX-COVER is applied with a putty knife on the cracked surface in one layer.

6. After the FLEX-COVER layer has dried, it is necessary to prime with FLEX-PRIMER and paint with FLEXCOAT.

Ready to work with our team?

Fill the form below to contact us and get your next project started!

About Us

 Our many years of experience, the quality, the wide range of products and brands, the distribution system, the support before and after the sale, the know-how, the service from our people, our unique showrooms, the Hadjiyiannis Academy and the investment in staff and our partners, all together compose the recipe of our success and the reason that for over half a century we build relationships of trust with you, our selected customers. 

Information